Pipa Baja Karbon API 5L Gr. B/X42 /X52 /X60 /X65 Psl2
| Fitur | Spesifikasi |
| Standar | API 5L PSL2 |
| Kelas | Gr. B / X42 / X52 / X60 / X65 |
| Jinis Pipa | Mulus / ERW / LSAW / SSAW |
| Diameter njaba | 1/2” – 60” (Bisa diatur) |
| Kekandelan Tembok | SCH 10 – SCH 160 |
| Dawane | 5.8m / 6m / 11.8m / 12m utawa Disesuaikan |
| Permukaan | Ireng / 3LPE / FBE / Galvanis |
| Saham | Inventaris Gedhe Kasedhiya |
| Rega | Pasokan Langsung Pabrik |
| Pangiriman | Pangiriman Cepet 15–30 Dina |
Pipa API 5LPipa baja karbon sing umum digunakake ing industri lenga lan gas. Pipa iki uga dadi sarana kanggo nggawa cairan liyane kaya ta uap, banyu, lan lendhut.
API 5L ditrapake kanggo pipa sing dilas lan pipa tanpa sambungan
Jinis-jinis sing dilas: Pipa ERW, SAW, DSAW, LSAW, SSAW, HSAW
Jenis-jenis pipa las API 5L sing umum yaiku kaya ing ngisor iki:
ERWLas tahanan listrik digunakake kanggo pipa kanthi diameter kurang saka 24 inci.
DSAW/ SAWPengelasan busur terendam dua sisi/pengelasan busur terendam minangka metode pengelasan liyane sing bisa digunakake minangka gantine ERW kanggo pipa diameter gedhe.
LSAWLas Busur Terendam Longitudinal digunakake kanggo pipa kanthi diameter nganti 48 inci. Dikenal minangka proses pembentukan JCOE.
SSAW/HSAW: Las busur terendam spiral/las busur terendam spiral kanthi diameter pipa nganti 100 inci.
Jinis Pipa Seamless: Pipa Seamless canai panas lan Pipa Seamless canai adhem
Pipa seamless biasane digunakake kanggo pipa diameter cilik (biasane kurang saka 24 inci).
(Pipa baja seamless luwih umum digunakake tinimbang pipa sing dilas kanggo diameter pipa kurang saka 150 mm (6 inci).
Kita uga nyedhiyakake pipa seamless diameter gedhe. Nggunakake teknik hot-rolling, kita bisa nggawe pipa seamless diameter nganti 20" (508 mm). Yen sampeyan butuh pipa seamless diameter luwih saka 20", kita bisa nggawe nganti 40" (1016 mm) diameter kanthi teknik hot-expanded.
API 5L nemtokake kelas ing ngisor iki: Kelas B, X42, X46, X52, X56, X60, X65, X70, lan X80.
Ana akeh macem-macem kelas baja kanggo pipa baja API 5L kayata Kelas B, X42, X46, X52, X56, X60, X65, X70, lan X80. Kanthi mundhake kelas baja, kontrol ekivalen karbon luwih ketat, kekuatan mekanik uga luwih dhuwur.
Uga, komposisi kimia pipa API 5L sing mulus lan dilas kanggo kelas tartamtu ora padha, pipa sing dilas duwe panjaluk sing luwih dhuwur lan jumlah karbon lan belerang sing luwih sithik.
Komposisi Kimia kanggo pipa PSL 1 kanthi t ≤ 0,984” | |||||||
| Kelas Baja | Fraksi massa, % adhedhasar analisis panas lan produk a,g | ||||||
| C | Mn | P | S | V | Nb | Ti | |
| maksimal b | maksimal b | maksimal | maksimal | maksimal | maksimal | maksimal | |
| Pipa Tanpa Seamless | |||||||
| A | 0.22 | 0.9 | 0.03 | 0.03 | – | – | – |
| B | 0.28 | 1.2 | 0.03 | 0.03 | c,d | c,d | d |
| X42 | 0.28 | 1.3 | 0.03 | 0.03 | d | d | d |
| X46 | 0.28 | 1.4 | 0.03 | 0.03 | d | d | d |
| X52 | 0.28 | 1.4 | 0.03 | 0.03 | d | d | d |
| X56 | 0.28 | 1.4 | 0.03 | 0.03 | d | d | d |
| X60 | 0.28 e | 1.40 e | 0.03 | 0.03 | f | f | f |
| X65 | 0.28 e | 1.40 e | 0.03 | 0.03 | f | f | f |
| X70 | 0.28 e | 1.40 e | 0.03 | 0.03 | f | f | f |
| Pipa sing dilas | |||||||
| A | 0.22 | 0.9 | 0.03 | 0.03 | – | – | – |
| B | 0.26 | 1.2 | 0.03 | 0.03 | c,d | c,d | d |
| X42 | 0.26 | 1.3 | 0.03 | 0.03 | d | d | d |
| X46 | 0.26 | 1.4 | 0.03 | 0.03 | d | d | d |
| X52 | 0.26 | 1.4 | 0.03 | 0.03 | d | d | d |
| X56 | 0.26 | 1.4 | 0.03 | 0.03 | d | d | d |
| X60 | 0.26 e | 1.40 e | 0.03 | 0.03 | f | f | f |
| X65 | 0.26 e | 1.45 e | 0.03 | 0.03 | f | f | f |
| X70 | 0.26e | 1.65 e | 0.03 | 0.03 | f | f | f |
| a. Cu ≤ = 0,50% Ni; ≤ 0,50%; Cr ≤ 0,50%; lan Mo ≤ 0,15%, | |||||||
| b.Kanggo saben pangurangan 0,01% ing ngisor kandungan karbon maksimum sing ditemtokake, kandungan mangan (Mn) sing diidinake bisa ditambah 0,05%, tundhuk karo watesan ing ngisor iki:Nganti 1,65% Mn kanggo kelas ≥ L245 (B) lan ≤ L360 (X52) Nganti 1,75% Mn kanggo kelas > L360 (X52) lan < L485 (X70) Nganti 2,00% Mn kanggo kelas L485 (X70) | |||||||
| c. Kajaba ana kesepakatan liya NB + V ≤ 0,06%, | |||||||
| d. Nb + V + TI ≤ 0,15%, | |||||||
| e. Kajaba ana kesepakatan liya., | |||||||
| f. Kajaba ana kesepakatan liya, NB + V = Ti ≤ 0,15%, | |||||||
| g. Ora ana tambahan B sing disengaja sing diidini lan B sing isih ana ≤ 0,001% | |||||||
| Komposisi Kimia kanggo pipa PSL 2 kanthi t ≤ 0,984” | |||||||||||||||||||||
| Kelas Baja | Fraksi massa, % adhedhasar analisis panas lan produk | Karbon sing padha karo | |||||||||||||||||||
| C | Si | Mn | P | S | V | Nb | Ti | Liyane | CE IIW | CE Pcm | |||||||||||
| maksimal b | maksimal | maksimal b | maksimal | maksimal | maksimal | maksimal | maksimal | maksimal | maksimal | ||||||||||||
| Pipa Mulus lan Dilas | |||||||||||||||||||||
| BR | 0.24 | 0.4 | 1.2 | 0.025 | 0.015 | c | c | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X42R | 0.24 | 0.4 | 1.2 | 0.025 | 0.015 | 0.06 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| BN | 0.24 | 0.4 | 1.2 | 0.025 | 0.015 | c | c | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X42N | 0.24 | 0.4 | 1.2 | 0.025 | 0.015 | 0.06 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X46N | 0.24 | 0.4 | 1.4 | 0.025 | 0.015 | 0.07 | 0.05 | 0.04 | d,e,l | 0.43 | 0.25 | ||||||||||
| X52N | 0.24 | 0.45 | 1.4 | 0.025 | 0.015 | 0.1 | 0.05 | 0.04 | d,e,l | 0.43 | 0.25 | ||||||||||
| X56N | 0.24 | 0.45 | 1.4 | 0.025 | 0.015 | 0.10f | 0.05 | 0.04 | d,e,l | 0.43 | 0.25 | ||||||||||
| X60N | 0.24f | 0.45f | 1.40f | 0.025 | 0.015 | 0.10f | 0.05f | 0.04f | g,h,l | Kaya sing wis disepakati | |||||||||||
| BQ | 0.18 | 0.45 | 1.4 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X42Q | 0.18 | 0.45 | 1.4 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X46Q | 0.18 | 0.45 | 1.4 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X52Q | 0.18 | 0.45 | 1.5 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X56Q | 0.18 | 0.45f | 1.5 | 0.025 | 0.015 | 0.07 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X60Q | 0.18f | 0.45f | 1.70f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X65Q | 0.18f | 0.45f | 1.70f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X70Q | 0.18f | 0.45f | 1.80f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X80Q | 0.18f | 0.45f | 1.90f | 0.025 | 0.015 | g | g | g | aku,j | Kaya sing wis disepakati | |||||||||||
| X90Q | 0.16f | 0.45f | 1.9 | 0.02 | 0.01 | g | g | g | j,k | Kaya sing wis disepakati | |||||||||||
| X100Q | 0.16f | 0.45f | 1.9 | 0.02 | 0.01 | g | g | g | j,k | Kaya sing wis disepakati | |||||||||||
| Pipa sing dilas | |||||||||||||||||||||
| BM | 0.22 | 0.45 | 1.2 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X42M | 0.22 | 0.45 | 1.3 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X46M | 0.22 | 0.45 | 1.3 | 0.025 | 0.015 | 0.05 | 0.05 | 0.04 | e,l | 0.43 | 0.25 | ||||||||||
| X52M | 0.22 | 0.45 | 1.4 | 0.025 | 0.015 | d | d | d | e,l | 0.43 | 0.25 | ||||||||||
| X56M | 0.22 | 0.45f | 1.4 | 0.025 | 0.015 | d | d | d | e,l | 0.43 | 0.25 | ||||||||||
| X60M | 0.12f | 0.45f | 1.60f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X65M | 0.12f | 0.45f | 1.60f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X70M | 0.12f | 0.45f | 1.70f | 0.025 | 0.015 | g | g | g | h,l | 0.43 | 0.25 | ||||||||||
| X80M | 0.12f | 0.45f | 1.85f | 0.025 | 0.015 | g | g | g | aku,j | .043f | 0.25 | ||||||||||
| X90M | 0.1 | 0.55f | 2.10f | 0.02 | 0.01 | g | g | g | aku,j | – | 0.25 | ||||||||||
| X100M | 0.1 | 0.55f | 2.10f | 0.02 | 0.01 | g | g | g | aku,j | – | 0.25 | ||||||||||
| a. SMLS t>0.787”, watesan CE kudu kaya sing disepakati. Watesan CEIIW sing ditrapake fi C > 0.12% lan watesan CEPcm ditrapake yen C ≤ 0.12%, | |||||||||||||||||||||
| b.Kanggo saben penurunan 0,01% ing ngisor kandungan karbon (C) maksimal sing ditemtokake, kandungan mangan (Mn) sing diidinake bisa ditambah 0,05%, ing watesan ing ngisor iki:Nganti 1,65% Mn kanggo kelas ≥ L245 (B) lan ≤ L360 (X52) Nganti 1,75% Mn kanggo kelas > L360 (X52) lan < L485 (X70) Nganti 2,00% Mn kanggo kelas ≥ L485 (X70) lan ≤ L555 (X80) Nganti 2,20% Mn kanggo kelas > L555 (X80) | |||||||||||||||||||||
| c. Kajaba ana kesepakatan liya Nb = V ≤ 0,06%, | |||||||||||||||||||||
| d. Nb = V = Ti ≤ 0,15%, | |||||||||||||||||||||
| e. Kajaba sarujuk, Cu ≤ 0,50%; Ni ≤ 0,30% Cr ≤ 0,30% lan Mo ≤ 0,15%, | |||||||||||||||||||||
| f. Kajaba ana kesepakatan liya, | |||||||||||||||||||||
| g. Kajaba ana kesepakatan liya, Nb + V + Ti ≤ 0,15%, | |||||||||||||||||||||
| h. Yen ora disepakati, Cu ≤ 0,50% Ni ≤ 0,50% Cr ≤ 0,50% lan MO ≤ 0,50%, | |||||||||||||||||||||
| i. Yen ora disepakati, Cu ≤ 0,50% Ni ≤ 1,00% Cr ≤ 0,50% lan MO ≤ 0,50%, | |||||||||||||||||||||
| j. B ≤ 0,004%, | |||||||||||||||||||||
| k. Yen ora disepakati, Cu ≤ 0,50% Ni ≤ 1,00% Cr ≤ 0,55% lan MO ≤ 0,80%, | |||||||||||||||||||||
| l. Kanggo kabeh kelas pipa PSL 2 kajaba kelas sing nganggo cathetan sikil j, ing ngisor iki ditrapake. Kajaba disepakati liya, ora ana tambahan B sing disengaja sing diidini lan B residual ≤ 0,001%. | |||||||||||||||||||||
| PSL1 | Kondisi Pangiriman | Kelas sing Ditrapake |
| Digulung, dinormalisasi, dibentuk normalisasi | A | |
| Digulung kaya biasane, digulung normalisasi, digulung termomekanis, dibentuk termo-mekanis, dibentuk normalisasi, dinormalisasi, dinormalisasi & ditemper, utawa yen disepakati, mung Q&T SMLS | B | |
| Digulung kaya biasane, digulung normalisasi, digulung termomekanis, dibentuk termo-mekanis, dibentuk normalisasi, dinormalisasi, dinormalisasi & ditemper | X42, X46, X52, X56, X60, X65, X70 |
| PSL2 | Kondisi Pangiriman | Kelas Pipa |
| Digulung | BR, X42R | |
| Normalisasi digulung/dibentuk, dinormalisasi, utawa dinormalisasi & ditemper | BN, X42N, X46N, X52N, X56N, X60N | |
| Dipateni & dipanasi | BQ, X42Q, X46Q, X56Q, X60Q, X65Q, X70Q, X80Q, X90Q, X100Q | |
| Termomekanik digulung/dibentuk | BM, X42M, X46M, X56M, X60M, X65M, X70M, X80M | |
| Termomekanik mung digulung | X90M, X100M, X120M | |
| Cathetan: Kanggo kelas PSL2, akhiran (R, N, Q, utawa M) minangka bagéan saka sebutan kelas baja. | ||
PSL1 lan PSL2 béda ing ruang lingkup pangujian uga ing sipat kimia lan mekaniké.
PSL2 luwih ketat tinimbang PSL1 ing komposisi kimia, sifat tarik, uji dampak, uji non-destruktif, lan liya-liyane.
Uji Dampak
Mung PSL2 sing mbutuhake uji dampak: kajaba X80.
NDT: Uji Non-Destruktif. PSL1 ora mbutuhake uji non-destruktif yen uji non-destruktif ora ditrapake. PSL2 mbutuhake.
(Pemeriksaan non-destruktif: Pengujian non-destruktif (NDT) lan pengujian NDT (nalika nggunakake prosedur pengujian NDT sing ditulis ing API 5L) yaiku aplikasi saka siji utawa luwih teknik pengujian non-destruktif kayata radiografi, ultrasonik (US), utawa liyane (sing materine ora dirusak) kanggo ngenali cacat lan ketidaksempurnaan ing pipa.)
Kemasan ikuumume wuda, pengikatan kawat baja, bangetkuwat.
Yen sampeyan duwe syarat khusus, sampeyan bisa nggunakakekemasan anti karat, lan luwih ayu.
Pancegahan kanggo pengemasan lan transportasi pipa baja karbon
1. Sajrone Transportasi & Panyimpenan
Pipa baja API 5Lkudu dilindhungi saka kejut, kompresi, pemotongan utawa kerusakan mekanik liyane sajrone pengepakan, transportasi, panyimpenan lan penanganan.
2. Praktik Penanganan sing Aman
Nalika sampeyan kerja barengpipa baja karbon, tansah njupuk pancegahan keamanan sing biasane kanggo nyegah kacilakan kayata bledosan, geni, utawa kena bahan kimia beracun.
3. Kondisi Layanan
Kowé ora kena tau nggunakakéPipa baja karbon API 5Ling suhu dhuwur, media korosif, utawa lingkungan abot liyane. Kanggo aplikasi kasebut, pilih pipa sing digawe saka kelas khusus sing tahan suhu dhuwur utawa korosi.
4. Pilihan Bahan & Spesifikasi
Nemtokake bahan lan kelas pipa sawise nimbang kanthi teliti kahanan operasi, kayata sifat lingkungan, jinis Media, tekanan lan suhu sarta aplikasi, lan liya-liyane.
5. Inspeksi & Pengujian Pra-Panggunaan
Baris Pope kudu dipriksa sadurunge digunakake kanggo ngonfirmasi kualitas lan kinerja.
Transportasi:Pangiriman Ekspres (Pangiriman Sampel), Udara, Rel, Darat, Laut (FCL utawa LCL utawa Curah)
P1: Jinis pipa sing kasedhiya?
A: Kita ngirim pipa seamless (SMLS), ERW, LSAW lan SSAW kanggo macem-macem aplikasi tekanan lan pipa.
Q2: Finishing lan lapisan permukaan endi sing bisa dipilih?
A: Lapisané 3LPE, FBE, dicet ireng utawa galvanis. Ana uga lapisan akhir pabrik normal.
Q3: Kepiye carane milih kelas pipa sing bener?
A: Pilih kelas miturut tekanan kerja, suhu, jinis medium lan kahanan sekitar. Yen sampeyan butuh, tenaga teknis kita bakal mbantu sampeyan milih kelas sing paling cocog kanggo proyek sampeyan.
Q4: Apa sertifikat kualitas sampeyan?
A: Kabeh Pipa Diprodhuksi miturut spesifikasi API 5L lan disedhiyakake karo MTC (Mill Test Certificate). Pipa PSL2 uga kudu ngalami pengujian lan inspeksi tambahan sing ketat.
Q5: Pira suwene wektu pangiriman?
A: Kanggo produk stok standar, wektu pangiriman bisa 7-20 dina gumantung saka ukuran, jumlah, lan tujuan.